ALLOY 625 PEPA IKE
Hoʻohui Kimia
Hoʻohui Kimia | Cr | Ni | Mo | Co | Cb+Ta | Al | Ti | C | Fe | Me | Mn | Si | P | S |
% Waiwai (ka liʻiliʻi) | 20.0 |
| 8.0 | - | 3.15 | - | - | - | - |
| - | - | - | - |
% Waiwai (kiʻekiʻe) | 23.0 | bal | 10.0 | 1.0 | 4.15 | 0.4 | 0.4 | 0.1 | 5.0 |
| 0.5 | 0.5 | 0.015 | 0.015 |
Na Waiwai Mechanical
Na Pono Mechanical & Kino | 21°C | 204°C | 316°C | 427°C | 538°C | 649°C | 760°C | 871°C |
ʻO ka ikaika ʻoi loa /Mpa | 992.9 | 923.9 | 910.1 | 910.1 | 896.3 | 820.5 | 527.8 | 275.8 |
0.2% Ka ikaika hua /MPa | 579.2 | 455.1 | 434.4 | 420.6 | 420.6 | 413.7 | 406.8 | 268.9 |
Elongation % | 44 | 45 | 42.5 | 45 | 48 | 34 | 59 | 117 |
Coefficient o ka hoonui wela um/moC | - | 13.1 | 13.3 | 13.7 | 14 | 14.8 | 15.3 | 15.8 |
ʻO ka hoʻoili wela /kcal/(hr.mc) | 8.5 | 10.7 | 12.2 | 13.5 | 15 | 16.4 | 17.9 | 19.6 |
Modulus o Elasticity/ MPa | 2.07 | 1.93 | 1.93 | 1.86 | 1.79 | 1.65 | 1.59 | - |
Nā noi
● Pūnaehana hoʻopau ʻenekini Jet
● Pūnaehana hoʻohuli ʻenekini
● Pūnaehana hoʻoheheʻe mokulele
● Nā apo puʻupuʻu turbine
● Bellows a me nā hono hoʻonui
● Nā ʻāpana wai kai
● mea hana kemika
Pale ʻino
Ua kū ʻo Alloy 625 i nā kaiapuni corrosive. Ma ka alkaline, ka wai paʻakai, ka wai hou, nā paʻakai kūʻokoʻa, a ma ka lewa, ʻaʻohe hoʻouka kaua. Hāʻawi ka nickel a me ka chromium i ke kū'ē i nā kaiapuni oxidizing. Hāʻawi ka Nickel a me ka molybdenum i ke kūʻē ʻana i nā lewa oxidizing.
Kāohi ʻia ka ʻino o ka lua a me ka ʻāʻī e ka molybdenum. Hoʻopaʻa ʻo Niobium i ka alloy e kū'ē i ka sensitization i ka wā wili. ʻOi aku ka maikaʻi o ke kūpaʻa ʻana o ke koʻikoʻi-corrosion ʻo Chloride. Kūleʻa ka alloy i ka scaling a me ka oxidation i nā wela kiʻekiʻe.
Inventory
PALAPALA HUA | KA NUI MAI | KA NUI IA |
Paipu huila 625 | 0.5 in | 8 in |
Alloy 625 coil | 0.25 mm | 3.18 mm |
Alloy 625 uwea wiliwili | 0.5 mm | 3.175 mm |
Alloy 625 pepa a me ka pā | 0.25 mm | 76.2 mm |
Alloy 625 pahu poepoe | 12 mm | 260 mm |
Alloy 625 paipu paipu | 0.5 in | 8 in |
Alloy 625 filanges | 0.5 in | 8 in |
Moʻomeheu Hui
Nā Waiwai Kūwaena: maikaʻi loa, ʻano hou, ʻoiaʻiʻo a lanakila-lanakila
Manaʻo lawelawe: E hana i ka waiwai no nā mea kūʻai aku, E hoʻomāʻona i nā mea kūʻai