HASTELLOY B2 UNS N10665 W.NR.2.4617
Hoʻohui Kimia
Alloy | ʻeleʻele | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Huina B2 | Min | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Kaulike | 1.0 | 30.0 | 2.0 | 1.0 |
Na Waiwai Mechanical
Kūlana Aolly | Ka ikaika tensile Rm Mpa Min | E hāʻawi i ka ikaika RP 0. 2 Mpa Min | ʻO ka lōʻihi A 5 % Min |
Hoʻoholo | 745 | 325 | 40 |
Na Waiwai Kino
ʻO ka mānoanoa g/cm3 | Lae hehee ℃ |
9.2 | 1330~1380 |
Kūlana
Rod, Bar, Uea, a me ka Lapa- ASTM B 335(Rod, Bar), ASTM B 564(Hoʻopaʻa ʻia), ASTM B 366(Kupono)
Papa, Pepa a me ka Strip- ASTM B 333
Paipu a Paipu- ASTM B 622(Hoʻoheheʻe ʻia) ASTM B 619/B626(Pūpepa Weled)
Nā hiʻohiʻona o Hastelloy B2
● Kū'ē nui i ke koʻikoʻi i ka pohā a me ka lua
● Kūʻē nui i ka hōʻemi ʻana i nā kūlana e like me ka hydrogen chloride, sulfuric, acetic a me ka phosphoric acids
● Kūʻē i ka waika hydrochloric ma nā ʻano a me nā mahana a pau
● Mua: INCONEL® alloy C-276 UNS N10276 / W.Nr. 2.4819
● Aʻe: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
No ke aha e koho ai iā mākou:
1. ʻOihana R&D hui
ʻO ke kākoʻo hoʻokolohua noi e hōʻoia ʻaʻole ʻoe hopohopo hou e pili ana i nā mea hana hoʻāʻo he nui.
2. Ka hui kūʻai huahana
Kūʻai ʻia nā huahana i nā ʻāina he nui a puni ka honua.
3. ʻO ka mana koʻikoʻi maikaʻi
4. Ka manawa hāʻawi paʻa a me ka mana o ka manawa hoʻouna kauoha kūpono.
He hui ʻoihana mākou, he nui nā makahiki o kā mākou mau lālā i ka ʻoihana kālepa honua. He hui ʻōpio mākou, piha i ka hoʻoikaika a me ka hana hou. He hui hoʻolaʻa mākou. Hoʻohana mākou i nā huahana kūpono e hōʻoluʻolu i nā mea kūʻai aku a lanakila i kā lākou hilinaʻi. He hui mākou me nā moeʻuhane. ʻO kā mākou moemoeā maʻamau ka hāʻawi ʻana i nā mea kūʻai aku i nā huahana hilinaʻi a hoʻomaikaʻi pū. E hilinaʻi iā mākou, lanakila-lanakila.