◆ ʻO Haynes-188 ka ikaika kiʻekiʻe kiʻekiʻe, ka anti-oxidation maikaʻi a me nā waiwai anti-corrosion, hoʻohana nui ʻia i ka aerospace, petrochemical, hana moku a me nā māla ʻē aʻe.

haku mele ʻana

Papa

C

Si

Mn

S

P

Cr

Ni

Fe

B

Co

W

La

ʻē aʻe

aole i oi aku mamua o

Haynes-188

0.05~0.15

0.2~0.5

1.25

0.015

0.02

21~23

20~24

≤3

≤0.015

40~45

13~15

0.03~0.15

-