Monel 400 Uns N04400 W.Nr. 2.4360 a me 2.4361
Hoʻohui Kimia
Alloy | ʻeleʻele | C | Si | Mn | S | Ni | Fe | Cu |
Monel 400 | Min | 63.0 | 28.0 | |||||
Max | 0.3 | 0.5 | 2.0 | 0.024 | 2.5 | 34.0 |
Na Waiwai Mechanical
Kūlana Aolly | Ka ikaika tensile Rm Mpa Min | E hāʻawi i ka ikaika RP 0. 2 Mpa Min | ʻO ka lōʻihi A 5 % Min |
Hoʻoholo | 745 | 325 | 40 |
Na Waiwai Kino
Kūlana Aolly | Ka ikaika tensile Rm Mpa Min. | Ka ikaika hua RP 0. 2 Mpa Min. | Elongation A 5 % |
i hoʻopili ʻia | 480 | 170 | 35 |
Kūlana
Rod, Bar, Uea, a me ka Lapa- ASTM B 164 (Rod, Bar, a me Wire),ASTM B 564 (Hoʻopaʻa ʻia)
Papa, Pepa a me ka Strip-,ASTM B 127, ASME SB 127
Paipu & Paipu- ASTM B 165(Hoʻoheheʻe ʻia a me ka Paipu ʻole), ASTM B 725 (Pipe Welded), ASTM B 730 (Pula Hoʻoheheʻe ʻia), ASTM B 751 (Pipe Welded), ASTM B 775 (Pipe Welded), ASTM B 829 (Pipe ʻole a me Paipu)
Huahana Welding- Metala Filler 60-AWS A5.14/ERNiCu-7;Welding Electrode 190-AWS A5.11/ENiCu-7.
Nā hiʻohiʻona o Monel 400
● Kūleʻa i ka wai kai a me ka mahu i nā wela kiʻekiʻe
● Kūleʻa maikaʻi loa i ka wai paʻakai a i ʻole ka wai kai
● Kūʻē maikaʻi loa i ka pohā ʻino ʻana i ka nui o nā wai hou
● Kūʻē kūʻē i nā waikawa hydrochloric a me nā waika hydrofluoric i ka wā e hoʻoneʻe ʻia ai
● Hāʻawi i kahi kūʻē i ka waika hydrochloric a me ka sulfuric i nā mahana haʻahaʻa a me nā haʻahaʻa haʻahaʻa, akā kakaikahi ka mea i koho ʻia no kēia mau waikawa.
● Kūʻē maikaʻi i ka paʻakai kūʻokoʻa a me ka paʻakai alkaline
● Ke kū'ē i ka chloride i hoʻoulu ʻia i ke koʻikoʻi ʻinoʻino
● ʻO nā waiwai mīkini maikaʻi mai nā mahana sub-zero a hiki i 1020° F
● Kū'ē kiʻekiʻe i ka alkali