ʻO ke kila kila ʻelua
Aluia Mahana Kiekie
◆F51 (31803) ʻo ia ka duplex stainless steel i hoʻohana nui ʻia, i hoʻohana nui ʻia i ka ʻaila ʻawaʻawa a me ka hoʻomaʻamaʻa kinoea, i ka hoʻomaʻemaʻe ʻana i ka aila, kemika, fertilizer, petrochemical a me nā māla ʻē aʻe, no ka hana ʻana i nā mea hoʻololi wela, condensing coolers, etc., ka mea i maʻalahi i ka luaʻi ʻana a me ke koʻikoʻi o ka ʻino o nā mea paʻi.Ma kahi o 304L, 316L austenitic stainless steel.
◆F53 (S32750) he super duplex stainless steel me ka nitrogen i hoʻohui ʻia, ka mea i hoʻohana nui ʻia i nā mea kemika, petrochemical a me nā mea moana e koi ai i ka ikaika kūikawā a me ka pale ʻana i ka corrosion.
◆F55 (S32760) mea he super duplex kuhiliʻole kila me ka ikaika kiʻekiʻe, kiʻekiʻe kū'ē i chloride localized corrosion a stress corrosion, a weldable.
ʻO ◆329 (S32900) maikaʻi ke kūpaʻa o ka oxidation, ka pale ʻana i ka corrosion, ka ikaika kiʻekiʻe, a kūpono hoʻi i nā wahi e like me ke kūpaʻa ʻana o ke kai.
◆A4 kila (0Cr17Mn13Mo2N) mea he lua-phase kila, a me kona corrosion kū'ē 'oi aku ka maikaʻi ma mua o ka hoʻohana mau austenitic kila me Mo maʻiʻo o 2% -3%.Hiki ke hoʻohana ʻia i nā mea kanu liʻiliʻi liʻiliʻi, nā lako urea piha, etc.
◆S31050 he kiʻekiʻe kū'ē i ka chloride stress corrosion māwae, maikaʻi kū'ē i pitting corrosion a crevice corrosion.
◆U3 he anti-scouring a me ka anti-corrosion waiwai, a ua hoʻohana pinepine ia e hana i ka valve cores, valve noho a me na mea e ae o loko.
Hoʻohana nui ʻia ʻo ◆HD i ka ʻoihana uila, ʻoihana photoelectric, ʻoihana petrochemical, ʻoihana kaʻa a me nā mea hoʻoponopono wikiwiki ʻē aʻe.
◆C4 kūpono no ka nui-scale vertical mixers, mixers, mixers, horizontal mixers a me nāʻoihana mīkini'ē aʻe.
◆DS-2 i corrosion kū'ē i ke kiʻekiʻe wela concentrated sulfuricʻakika, a ua kūpono no ka mīkini 'oihana i kiʻekiʻe wela concentrated sulfuricʻakikaʻoihana.
haku mele ʻana
Papa | C | Si | Mn | S | P | Cr | Ni | Mo | Cu | N | W | ʻē aʻe |
aole i oi aku mamua o | ||||||||||||
F51 | 0.03 | 1 | 2 | 0.02 | 0.03 | 21~23 | 4.5~6.5 | 2.5~3.5 | - | 0.08~0.2 | - | - |
F53 | 0.03 | 0.8 | 1.2 | 0.02 | 0.035 | 24~26 | 6~8 | 3~5 | ≤0.5 | 0.24~0.32 | — | - |
F55 | 0.03 | 1 | 1 | 0.01 | 0.03 | 24~26 | 6~8 | 3~4 | 0.5~1 | 0.2~0.3 | 0.5~1 | - |
329 | 0.08 | 1 | 1.5 | 0.03 | 0.035 | 23~28 | 3~6 | 1~3 | - | - | - | - |
A4 kila | 0.08 | 0.7 | 12~15 | 0.02 | 0.045 | 16.5~18.5 | - | 1.8~2.2 | - | 0.2~0.3 | - | - |
S31050 | 0.02 | 0.7 | 2 | 0.01 | 0.025 | 24~26 | 21~23 | 2~2.5 | — | 0.1~0.16 | — | - |
U3 | 0.02 | 0.4 | 2.5~3 | 0.015 | 0.02 | 24~26 | 19~21 | 2.5~3 | — | 0.2~0.3 | - | - |
HD | 0.03 | 4.5~6 | 1 | 0.01 | 0.03 | 17~19 | 18~20 | 0.3~0.8 | 1.5~2.5 | - | - | - |
C4 | 0.03 | 3~4.5 | 1 | 0.025 | 0.03 | 13~15 | 13~15 | - | - | - | - | - |
DS-2 | 0.02 | 5~7 | 1 | 0.03 | 0.03 | 8~11 | 22~25 | - | - | - | - | - |
ʻO ka liʻiliʻi o ka waiwai huila
mokuʻāina | ikaika uʻi RmN/m㎡ | Ka ikaika o ka hua Rp0.2N/m㎡ | Elongation As% | Brinell paakiki HB | |
F51 | Lapaʻau hoʻonā | 620 | 450 | 25 | 290 |
F53 | Lapaʻau hoʻonā | 800 | 550 | 15 | 310 |
F55 | Lapaʻau hoʻonā | 820 | 550 | 25 | - |
329 | Lapaʻau hoʻonā | 620 | 485 | 20 | 271 |
A4 kila | Lapaʻau hoʻonā | 480 | 255 | 25 | - |
S31050 | Lapaʻau hoʻonā | 650 | 380 | 24 | - |
U3 | Lapaʻau hoʻonā | 680 | 400 | 22 | - |
HD | Lapaʻau hoʻonā | 750 | 410 | 25 | - |
C4 | Lapaʻau hoʻonā | 800 | 400 | 23 | - |
DS-2 | Lapaʻau hoʻonā | 690 | 390 | 21 | - |