Monel
Aluia Mahana Kiekie
◆Monel400 loaʻa i ka corrosion kū'ē maikaʻi i ka hydrofluoric acid a me ka fluorine kinoea, a he kūpono no ka paipu paipu a me nā kiwikā i hoʻohana 'ia i loko o ka oihana kemika, ka aila, atomic ikehu, a me ka hooulu moana.
◆ʻO Monel500 he mau waiwai mechanical piha maikaʻi, ikaika kiʻekiʻe a me ke kū'ēʻana i ka corrosion.He kūpono ia no nā mea hoʻopaʻa a me nā ʻāpana hana i hoʻohana ʻia i ka ʻoihana kemika, nā moku a me nā ʻenehana moana.
◆ Hoʻohana nui ʻia ʻo Monel404 i ka petrochemical, ʻoihana nuklea, a me nā mea ʻenehana ʻokiʻoki ʻē aʻe.
haku mele ʻana
Papa | C | Si | Mn | S | P | Cr | Ni | Mo | Fe | Co | W | Al | Ti | Cu |
aole i oi aku mamua o | ||||||||||||||
Monel400 | 0.3 | 0.5 | 2 | 0.024 | - | - | kumu | - | ≤2.5 | - | - | - | - | 28~34 |
Monel500 | 0.18 | 0.5 | 1.5 | 0.01 | - | - | ≥63 | - | ≤2 | - | - | 2.3~3.15 | 0.35~0.85 | 27~33 |
Monel404 | 0.15 | 0.1 | 0.1 | 0.024 | - | - | 52~57 | - | ≤0.5 | - | - | ≤0.05 | - | Noho |
ʻO ka liʻiliʻi o ka waiwai huila
Papa | Kūlana ʻenehana | ikaika uʻi RmN/m㎡ | Ka ikaika o ka hua Rp0.2N/m㎡ | Elongation As% | Brinell paakiki HB |
Monel400 | ʻOlokaʻi ʻia/wela ʻia | 516 | 170 | 35 | - |
Mokuʻāina Annealed | 483 | 170 | 35 | - | |
Monel500 | Kūlana hoʻopunipuni + ʻelemakule | 960 | 686 | 20 | 27 |
paʻa paʻa + ʻelemakule | 896 | 585 | 20 | 24 | |
Monel404 | Mokuʻāina Annealed | 550 | 185 | 36 | - |